Does anyone know any website which can cross-reference DIN material to ASTM designation?

I have some DIN material such as 1.0254, 1.4310 etc, and need to know the ASTM designation.

Thank you in advance.
 
Replies continue below

Recommended for you

Dear Fawkes,

I have tried matweb but do not have any luck. Thanks for response.
 
P+V,

If I remember correctly,

1.4310 (X 12 CrNi 17 7) is equivalent to AISI 301
1.0254--- NO information.

Hope this helps.