Hi All,
I hope someone here can help. We're trying to clean up some metalograph samples at our local university and I need some cross qualification info for the following alloys.
Base Metals
BS 4360 gr 1 mild steel (.18% C)
BS 970 grade En8 (.4% C)
BS 2870 grade C101 (Tough-pitch Cu)
BS 2870 grade C106 (Phos-deoxidised Cu)


Welding Electrodes
BS 1719 class 3 (CS)
BS 1719 class 6 (CS)

Thanks for any info
Koz
 
Replies continue below

Recommended for you

BS 4360 is an obsolete spec, so I would need a more contemporary BS or BS EN standard number for that grade. EN 8 is equivalent to SAE 1042 according to SAE J403. You can find information on the copper alloys at the CDA website:

 
Hi all,

The BS specs I mentioned have been broken up into about 10 specs in the new BS nomenclature. I, of course, was looking for an easy way out. I think I'll ref AISI for the U. Thanks for all of your help.

Koz
 
FYI, AISI no longer maintains standards for steel chemical compositions. SAE and ASTM do.
 
Hi TVP,

I am old school! I'll try to catch up

Koz
 