Jun 13, 2002 #1 Rafi12 Mechanical Joined Jun 11, 2002 Messages 5 Location US I would like to know the creep crack growth properties of CrMoV. what is the best source that could give me this information?
I would like to know the creep crack growth properties of CrMoV. what is the best source that could give me this information?
Jun 17, 2002 #2 tedg Materials Joined Dec 23, 2000 Messages 34 Location US Rafi: Would suggest you read the chapters on crack initiation and growth in "Fracture & Fatigue Control in Structures" by Barsom & Rolfe; published by Prentice & Hall. ISBN 0-13-329863-9 025. Upvote 0 Downvote
Rafi: Would suggest you read the chapters on crack initiation and growth in "Fracture & Fatigue Control in Structures" by Barsom & Rolfe; published by Prentice & Hall. ISBN 0-13-329863-9 025.
Jul 3, 2002 #3 GordonF Materials Joined Jul 3, 2002 Messages 16 Location US Rafi BS7910:1999 appendix U has constants for creep crack growth estimation for a number of materials including CrMoV. Upvote 0 Downvote
Rafi BS7910:1999 appendix U has constants for creep crack growth estimation for a number of materials including CrMoV.