I would like to know the creep crack growth properties of CrMoV. what is the best source that could give me this information?
 
Replies continue below

Recommended for you

Rafi:

Would suggest you read the chapters on crack initiation and growth in "Fracture & Fatigue Control in Structures" by Barsom & Rolfe; published by Prentice & Hall.
ISBN 0-13-329863-9 025.
 
Rafi

BS7910:1999 appendix U has constants for creep crack growth estimation for a number of materials including CrMoV.
 