Hi,
Was wondering if its possible to weld CREUSABRO 4800 to ST-37?
The final weld seam isnt subjected to high loads.
Chemical compositions listed below are for max values and in % by mass.
CREUSABRO 4800: C - 0.20, Mn - 1.6, Ni - 0.20, Cr - 1.9, Mo - 0.4, S - 0.005, P - 0.018
ST-37: C - 0.17, Mn - 1.4, P - 0.045, S - 0.45
Thanks.
Was wondering if its possible to weld CREUSABRO 4800 to ST-37?
The final weld seam isnt subjected to high loads.
Chemical compositions listed below are for max values and in % by mass.
CREUSABRO 4800: C - 0.20, Mn - 1.6, Ni - 0.20, Cr - 1.9, Mo - 0.4, S - 0.005, P - 0.018
ST-37: C - 0.17, Mn - 1.4, P - 0.045, S - 0.45
Thanks.