I would like to better understand how ASME VIII-1 and EN13445 consider creep design. For example, if I have a vessel in SA 516 Gr.70 (tabulated for creep from about 370 °C) with a design temperature of 400 °C, but the customer confirms to us that the equipment does not work under creep conditions because the operating temperature is 300 °C. How do the two codes deal with these cases?

Thank you in advance
 
Just to better understand your question, what do you mean by "deal with"?
 
Based on the topics title, my first answer would be that ASME VIII-1 fat better addresses creep (materials properties, design rules, etc.) than EN 13445. Especially above 600 deg C EN 13445 is just lacing details.

But then your question is far different, so what exactly are you looking for?

Huub
- You never get what you expect, you only get what you inspect.
 
FPPE,
The question is if the operating temp is 300C, how did you set the design temp as 400? It s too big margin.

If you set the design temperature correctly, you will not fall into the creep as per stress Table 1A for SA-516 Gr 70.

GDD