Crazing in hard coat anodize

Status
Not open for further replies.

botrott

Mechanical
Jan 20, 2009
2
Does anyone know the affect crazing in hard coat anodize will have if the parts are put through environmental testing such as humidity and salt & fog? Also, if the crazing occurs in a vacuum surface will it cause leaks.
 
Replies continue below

Recommended for you

If the crazing occurs on a seal surface then it could be a source of leaks. What type of aluminum and why do you need to hard anodize?
 