- Feb 27, 2002
- 4
HELP!!
Hi, They poured my slab on Feb 26, one day later there were several cracks 15 to 25 feet long. One was almost 1/8" wide. I know concrete can crack but like this? When they poured it it was sunny and 70, that evening it went down into the 40's. I am really concerned there is more of a problem then just shrinkage. What can be done to repaor this. The builder says "this is normal". The slab they poured the previous Friday does not have a single crack.
What should be done?
John
Hi, They poured my slab on Feb 26, one day later there were several cracks 15 to 25 feet long. One was almost 1/8" wide. I know concrete can crack but like this? When they poured it it was sunny and 70, that evening it went down into the 40's. I am really concerned there is more of a problem then just shrinkage. What can be done to repaor this. The builder says "this is normal". The slab they poured the previous Friday does not have a single crack.