XR250
Structural
- Jan 30, 2013
- 5,988
I am still unclear on this issue. I am working on a metal stud job where I am using epoxy anchors in various situations. Many are for a cantilevered sill, so I have one bolt at each stud (16" O.C.) and it acts in tension only (about 1400 lbs ASD). This is an existing building with 9" PT slabs. They are going to x-ray it to make sure we don't hit anything.
If I assume cracked concrete, my anchor fails unless we go with a deeper embedment. If I assume un-cracked, it passes.
I have asked a few former collegues and they say they would assume un-cracked.
What are the rules?
If I assume cracked concrete, my anchor fails unless we go with a deeper embedment. If I assume un-cracked, it passes.
I have asked a few former collegues and they say they would assume un-cracked.
What are the rules?