Crack under riser - thread330-213484

Status
Not open for further replies.

RAJMETALLURGY

Materials
Dec 1, 2010
33
What is the solution for the earlier thread "thread330-213484" regarding under riser crack in carbon steel.
Please some one guide me.
 
Replies continue below

Recommended for you

Start a new thread and state your problem. Do not refer to nearly 10 years old thread. Taking a clue from the referenced thread,, please state the steps you have taken.