We have subcontracted installation of CP system for 6 nos. above ground crude oil tanks. since 18 months 4 of the 6 tanks are completed and handed over to the client but we are facing a problem of final acceptance and partial completion of the project since the CP system is not giving proper results using the measurement of the Test posts. The system is impressed current CP system using mesh anode distribution below the tank bottom (60m dia.) and connected to rectifier 125A at 24Volt. design current is 90A and the system is not getting polarized to -ve 800mV requirement. the subcontractor is giving us the reason for that is because of the bottom plate is not painted. But it was a requirement for impressed current CP bottom to be bare and the design is based on that.
anyone has faced similar situation?
anyone has faced similar situation?