Dear All,
Can anyone inform if galvanic corrosion could take place when coupling CS RTJ Flanges with super austenitic SS (904 L) ring joints in sea water environment ?

Regards
 
Yes, and the corrosion of the CS is all that will keep the 904L from corroding.
It is not a seawater suitable alloy.

= = = = = = = = = = = = = = = = = = = =