There are a dozen vendors and I would guess that $15-40k would get you one.
Price will depend on a few things, sample size, resolution, max temp, heating and cooling rates, gases and flow controls, and so on.
Some of these are built to use small samples (~100mg) and some will handle 5g samples.
Lots of options.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed