Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Cost Estimate for FRP Laminate installation and near surface mounted FRP rod/bar installation?

Status
Not open for further replies.

b52oc

Civil/Environmental
Joined
Sep 25, 2014
Messages
1
Location
US
I'm just looking for a ballpark figure for square foot cost for labor and materials for retrofitting unreinforced masonry (URM) walls with externally bonded FRP laminates and perhaps a per linear foot labor and material cost for retrofitting URM walls with NSM FRP rods. Can anyone get me in the ballpark? Thanks!
 
I assume this for the US?

For CMU with surface-mounted wet-layup FRP ballpark cost (material supply and labor install) is $25/SF based upon prepared surface area. Assuming FRP is carbon.

Above price does not include any fire-related coating for smoke-developed or flame-spread, nor fire resistance.

For NSM pultruded bars varies depending if glass or carbon is used. I am a bit out of touch with current pultruded bar pricing so I cannot help you there.
 