I'm looking for design information for corrugated steel water tanks subject to wind, snow, and seismic loads. I have been asked to do some work for a tank manufacturer. These have a bolted corrugated steel wall, no bottom, and a plastic liner. Size say 14m dia and 2.4m high. These are common as farm tanks.

I am familiar with API 650 and AWWA D100 but these don't cover corrugated steel.

Do you know of any information relevant to corrugated steel?
 
Replies continue below

Recommended for you

You could have a look at AS 2304, covering water storage tanks for fire protection systems. These are typically bolted corrugated tanks.
 

Your approach should be a hybrid approach.

Regarding bolted joint design apply the AISC code .

For seismic , wind design you may look API 650 or AWWA and ASCE 7-16 ( 15.7 TANKS AND VESSELS ).

For a specific case, if you provide dia, height, roof type ( or open top ),and content you may get specific responds.
 
Thanks BJI, that looks like what I need.
 