And some chloride road-salts are worse than others. Sodium chloride at least will dry out, and corrosion attack will be reduced on dry days. Calcium chloride is highly hygroscopic and never truly dries out, so it never ceases its' attack on your car. Or, in the words of Neil Young, "Rust never sleeps."