Jun 27, 2016 #1 chimieindustrielle Chemical Joined Sep 18, 2015 Messages 12 Location TN Dear friends; In the presence of H2S ,CO2 and water in the gas : Does corrosion and crystal formation occurs together ? Best Regards !
Dear friends; In the presence of H2S ,CO2 and water in the gas : Does corrosion and crystal formation occurs together ? Best Regards !
Jun 28, 2016 #2 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA Corrosion of what, steel? It depends on temperature and the amount of water. If there is liquid you can get different results. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
Corrosion of what, steel? It depends on temperature and the amount of water. If there is liquid you can get different results. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Jun 29, 2016 #3 SJones Petroleum Joined Apr 22, 2001 Messages 3,944 Location GB Does "crystal formation" mean gas hydrate formation? Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
Does "crystal formation" mean gas hydrate formation? Steve Jones Corrosion Management Consultant http://www.linkedin.com/pub/8/83b/b04 All answers are personal opinions only and are in no way connected with any employer.