Inspector_1998
Mechanical
Recently I have observed CUI at several locations Upstream/downstream of expansion loops of pipelines especially: lower section of pipelines between 4 to 5 clock position) and the length of a corroded area less than a half meter along of the pipelines that marked on the attached image.
the constructed material is Carbon steel and size starting from 8 inches to 18''.
Now, what are the possible solution to stop the further corrosion build up? Since these lines are not coated.
Also, what
thickness measurement carried out and found the remaining thickness as under
18'' Schedule 30 (NT 11.1mm), operating temperature 95C = 5.4mm ( actual remaining thickness) advance CUI stage
12'' Schedule 30 (NT 8.38mm), operating temperature 45C = 5.1mm ( actual remaining thickness) Med.CUI stage.
8'' Schedule 30 (NT 7.04mm), operating temperature 45C = 5.2mm ( actual remaining thickness) Intial CUI stage.
THE INSULATION TYPE: Rockwool insulation.
the affected type has been highlighted in the attachment.
I am looking for the temporary repair since these lines can 't be isolated due operational needed.