Would a 65Mn lasts long in a corrosive environment like geothermal field with the presence of H2S? Is it inferior or superior in corrosion resistance properties compared to 316 stainless steel?

Thanks,
Robert Guazo
Instrumentation Design Engineer
 
Replies continue below

Recommended for you

65Mn would not lasst long in a corrosive environment. It would be inferior to 316 stainless steel.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Hi! Do you have any reference for the material composition of Mn65? Thanks!
 