Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Corrosion Resistance Properties of 65Mn 1

Status
Not open for further replies.

exodus02

Electrical
Joined
Jul 29, 2008
Messages
3
Would a 65Mn lasts long in a corrosive environment like geothermal field with the presence of H2S? Is it inferior or superior in corrosion resistance properties compared to 316 stainless steel?

Thanks,
Robert Guazo
Instrumentation Design Engineer
 
65Mn would not lasst long in a corrosive environment. It would be inferior to 316 stainless steel.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Hi! Do you have any reference for the material composition of Mn65? Thanks!
 