Corrosion resistance of Inconel 718, Inconel X750 and Incoloy A286 with dilute sulphuric acid at 70C

Status
Not open for further replies.

ballvalveguy

Petroleum
Joined
May 12, 2007
Messages
30
Location
US
I am aware that these three metals are not great with sulphuric acid, but I need to specify a spring material that will work in this application. I picked what I consider to be probably the best choices, but if anyone can give me some insight in to which would be the best material to use, I'd appreciate it.
 
How dilute?
Have you gone to the Special Metals web site and looked at the data sheets for these alloys?

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 
NiDI

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 