Jul 13, 2007 #1 dsnyder2 Materials Joined Jul 11, 2007 Messages 7 Location US Does anybody know where I could access a free database for corrosion rates for common iron alloys (I need stainless steel AISI 304 and 316, and carbon steel ASTM A516, corrosion rates for sulfonic acid)
Does anybody know where I could access a free database for corrosion rates for common iron alloys (I need stainless steel AISI 304 and 316, and carbon steel ASTM A516, corrosion rates for sulfonic acid)
Jul 13, 2007 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Go here for starters http://www.outokumpu.com/applications/documents/start.asp Upvote 0 Downvote
Jul 13, 2007 Thread starter #3 dsnyder2 Materials Joined Jul 11, 2007 Messages 7 Location US exactly what im looking for, but does not have sulfonic acid. Maybe this is because R values for sulfonic chain vary, and thus corrosion varies? Upvote 0 Downvote
exactly what im looking for, but does not have sulfonic acid. Maybe this is because R values for sulfonic chain vary, and thus corrosion varies?
Jul 13, 2007 #4 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US I checked on an on line subsciber service which provides access to the Corrosion Survey Database by NACE, and I could not locate sulfonic acid. Upvote 0 Downvote
I checked on an on line subsciber service which provides access to the Corrosion Survey Database by NACE, and I could not locate sulfonic acid.
Jul 13, 2007 #5 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA Isn't sulfonic actually a mixture of various compounds? Do you know anyone that is a member of MTI? It might be in their corrosion data book. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm Upvote 0 Downvote
Isn't sulfonic actually a mixture of various compounds? Do you know anyone that is a member of MTI? It might be in their corrosion data book. = = = = = = = = = = = = = = = = = = = = Rust never sleeps Neither should your protection http://www.trent-tube.com/contact/Tech_Assist.cfm