Hi,

I'm looking for a corrosion chart or table where corrosion rate of AISI 304L in Methanol (Methylic Alcohol)is analised.

I have to design the piping of methanol transport and i would like to know the anual corrosion rate for methanol at, at least, 130ºC, 2,5 bar (absolute).

Thank you
 
Replies continue below

Recommended for you

yhisus,
Try visit the OutoKumpu's website and order your Corrosion Handbook ninth edition. It's free and is valued in gold...
SA 304/304L is good, but you could also consider the cheaper 13%Cr corrosion resistant steels.