ootpik

Mechanical
Dec 23, 2005
3
How is the corrosion rate of AISI 1026 effected by acid concentration, specifically comparing corrosion rate in a 15% HCl enviroment to a 28% HCl environment?
 
Replies continue below

Recommended for you

Either HCl concentration will quickly destroy AISI 1026.

The corrosion rate is so high as to be meaningless.
 