Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Corrosion of galvanised steel nuts and bolts in Al Bronze casting

Status
Not open for further replies.

sayee1

Materials
Joined
Feb 6, 2003
Messages
281
Location
SA
The subject materials(SA193 B7bolts, B148C95800 Al Bronze casting) intended for valve for seawater service. The galvanised nuts are not coming into contact with the seawater(They are on the side of the casting not in contact with sea water). In that case is any insulation required between the Al bronze and the galvanised nuts? Is this combination of nuts and casting ok?

Thanks and regards
Sayee Prasad R
Ph: 0097143968906
Mob: 00971507682668
End of all knowledge is the attainment of immortality!
 
Doesn't sound to me like you have a corrosion concern here. The Zn should protect against atmospheric humidity very well-Zn is quite good because scratches etc. in it don't affect the protection much.

I also don't see any problem with the bronze side either. But all this changes if sea water gets involved.
 