Does anyone know what is involved with the inspection and evaluation of the interior corrosion resistant C-276 linings of the duct for the Flue Gas Desulphurization systems and the testing equipment/instruments that may be necessary or where that information may be found?

Thank you;

Russ A. Fleming
russ.fleming@lambertengineers.com




 
The inspections should be focused on conditions that would present a concern. These might be leakage, pitting corrosion, cracking of welds, etc. I would start with a good visual inspection of all accessible surfaces for evidence of pitting, weld cracking, staining that might indicate areas of leakage, corrosion/wastage of base material, etc. You might pressurize the system and do a leakage test with a soapy solution on welds or connections. If you see any pitting corrosion, you might measure the depth of the pits. These are all just common sense areas of inspection. Don't make it harder than it needs to be.
 