We are having some corrosion issues with Duplex stainless steel grade 2205 piping used in the Gulf region for a sea water cooling process. We are yet to find the root cause of the corrosion and are presently investigating if it is a welding problem, or a problem with the material selection generally.
We have reference of other projects in the area using corrosion inhibitor dosing at the sea water inlet.
Does anyone have any experience to share of duplex 2205 corrosion in Gulf seawater, and use of corrosion inhibitors?
Thanks,
Tom
We are having some corrosion issues with Duplex stainless steel grade 2205 piping used in the Gulf region for a sea water cooling process. We are yet to find the root cause of the corrosion and are presently investigating if it is a welding problem, or a problem with the material selection generally.
We have reference of other projects in the area using corrosion inhibitor dosing at the sea water inlet.
Does anyone have any experience to share of duplex 2205 corrosion in Gulf seawater, and use of corrosion inhibitors?
Thanks,
Tom