what inhibitor type are suitable injected in gas transmission containing high CO2 & no H2S? What is multi injection and are there any effect?
--thx 4 ur advice--
Hi xda! excuse my english
in our experience use filmogene and neutralizing product
use product based on aliphatics( fats) amins (80%) and lights amins 20%( neutralisor)