It depends on the inhibitor.
Talk to your supplier.
In many cases even if there is carryover it will not be effective.
Many inhibitors have a rather narrow range of use (temp, pH, TDS, ...) and it may not be suitable.
Some have virtually no carryover, while some are more volatile and will carryover a lot.
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed