Recently came across high corrosion in an underground fire ring main of MS construction(no coating) that runs on top of a mains electrical cable feeding the site.My understanding is that stray currents caused by a DC field can cause corrosion in pipe lines.Can an AC field cause corrosion in pipe lines?
 
In a word, yes.


"You see, wire telegraph is like a very long cat. You pull his tail in New York and his head is meowing in Los Angeles. Do you understand this? Radio operates the same way: You send signals here, they receive them there. The only difference is there is no cat." A. Einstein
 
any stray currents can cause accelerated corrosion.
These should be treated like natural gas lines, OD coatings and cathodic protection.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Unless your pipe is way out in the middle of nowhere, you can assume there will be some stray current.
 