petrotrinsmerv
Chemical
We upgraded a small vacuum column (26,000 BPSD) a few years ago and changed the overhead from direct contact ejector condensers to shell and tube ejector condeners. We are experiencing severe corrosion problems due to low sour water pH problems (column uses stripping steam). Can we use ahhydrous Ammonia here. The current thinking is that if we can condense water, enough of the Ammonia will partition into the condensed sour water (26 inHg vacuum)to raise the pH. Is this wishful thinking?