Hi Everyone ,
AD2000 B0 9.2.1 says you have to add 1 mm corrrosion allowance if you are using carbon steel .. But İM not sure is that neccesary? For example im designing an lpg or air tank t<30 mm and will be painted just from outside ( no protection from inside) am i have to add 1 mm corrosion allowance to min . thickness ? sometimes our customers wants vessel with carbon steel with 0 mm corrosion allowance ( no protection from inside ) is it imposible for AD2000?
AD2000 B0 9.2.1 says you have to add 1 mm corrrosion allowance if you are using carbon steel .. But İM not sure is that neccesary? For example im designing an lpg or air tank t<30 mm and will be painted just from outside ( no protection from inside) am i have to add 1 mm corrosion allowance to min . thickness ? sometimes our customers wants vessel with carbon steel with 0 mm corrosion allowance ( no protection from inside ) is it imposible for AD2000?