Gent.
We have Water Oil Separator equipment in the plant, and there are some relief valves in the gas & liquid sides.
We have a problem with a repetitive corrosion in the relief valves annually, every time we dismantle the relief valve the inspection revealed a highly corrosive rate. (196 MPY). The body material is carbon steel & we cannot utilize stainless steel due to carbonate.
Our usual treatment methods are as following:
• Preheat.
• Grinding.
• Remove the defected materials.
• Welding overlay.
• Coating (APCS-2A & APCS-114).
I am wondering if there is any solution to reduce the corrosion rate, can we utilize rapture disc / line relief or other methods?
Please help if you face this situation before and you know away to resolve it.
Your quick & active response will be highly appreciated.
I am always ready for help as much as i can .. so just let me know your Problem .
We have Water Oil Separator equipment in the plant, and there are some relief valves in the gas & liquid sides.
We have a problem with a repetitive corrosion in the relief valves annually, every time we dismantle the relief valve the inspection revealed a highly corrosive rate. (196 MPY). The body material is carbon steel & we cannot utilize stainless steel due to carbonate.
Our usual treatment methods are as following:
• Preheat.
• Grinding.
• Remove the defected materials.
• Welding overlay.
• Coating (APCS-2A & APCS-114).
I am wondering if there is any solution to reduce the corrosion rate, can we utilize rapture disc / line relief or other methods?
Please help if you face this situation before and you know away to resolve it.
Your quick & active response will be highly appreciated.
I am always ready for help as much as i can .. so just let me know your Problem .