I face problem of delamination between foam (corecell-M) and prepreg (45% of epoxy). I believe that delamination problem came from contamination. I would like to fing a way to clean foam before wrapping with prepreg. During machining, chip of foam are create. A lot of dust stay on the foam and ensure a bad adhesion during curing. I would like to eliminate those foam chip by a chemical way. Can you suggest me products to use for cleaning (surface preparation) then avoid chemical reaction with the foam. Can you gieve me some ideas?
I will also try other type of foam (corecell-A) to see if it will reduce the amount of foam chip (more easy tom machine).
etchac
I will also try other type of foam (corecell-A) to see if it will reduce the amount of foam chip (more easy tom machine).