Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Copper Vs Stainless Steel in an Earth Mat

Status
Not open for further replies.

mpnes

Electrical
Jul 11, 2005
3
Hi there,

I have a bit of a dilemma. My supervisor just returned from Germany and while he was there he discovered that on Cell Sites they use stainless to form a ring with electrodes to earth the mast. Has anyone out there know any pros and cons of using stainless over copper.

Thx in advance
 
Replies continue below

Recommended for you

copper- cheaper, good conductivity, easy to weld in the field, common grounding material.

Stainless- well, can't think of a reason to use it other than corrosion.

JTK
 
Galvanized strip is common in Europe. A lot of copper in the ground may cause problems with galvanic corrosion of galvanized steel buried nearby.
 
Do a google search and read up on stress corrosion. Stainless can corrode in different modes. Copper corrodes uniformly over the entire area of the matt or ground rod. Stainless can corrode between the grains of the metal and develope cracks ( stress corrosion). Stainless is pretty but not allways the best choice for ground mats or rods. You've got homework.
 