Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Copper Nickel plate (UNS 71500) - NACE MR 0175-

Status
Not open for further replies.

jerin james

Mechanical
Sep 17, 2020
30
Dear Sirs,

Good day all.

Is restrictions/requirements on Copper Nickel plate (UNS 71500) covered under NACE MR 0175. If yes, kindly advise.

Thanks
Jerin James
 
Replies continue below

Recommended for you

There are no restrictions, but it is pointed out that there could be issues with general corrosion in H2S containing fluids.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
Velocity, if fluids are present CuNi has very strict velocity limitations.
 