Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Copper Content in SA-182 F316L Flanges – Compliance and Concerns

Status
Not open for further replies.

Ehsan.m

Mechanical
Joined
Aug 12, 2024
Messages
2
Location
CA
Hello everyone,

I recently received a batch of SA-182 F316L stainless steel flanges at my company. Upon reviewing the Material Test Reports (MTRs), I noticed that these flanges contain copper, which is not typically listed as a standard element in the chemical composition for F316L according to ASME BPVC Section II.A.

My questions are:

Has anyone else encountered F316L flanges with copper content? If so, was this considered acceptable under ASME standards or did it raise compliance concerns?
Could the presence of copper affect the performance of these flanges, particularly in high-temperature or corrosive environments, which F316L is usually designed to withstand?
Is this a known issue with certain suppliers or manufacturers, and how have others in the industry handled similar situations?
I would appreciate any insights or experiences you can share regarding this issue. I want to ensure that the materials we use fully comply with ASME standards and do not compromise the safety or integrity of our systems.

Thank you!
 
"Has anyone else encountered F316L flanges with copper content?" NO

any MTR that i reviewed and did not comply with the standard was rejected.

"Is this a known issue with certain suppliers or manufacturers, and how have others in the industry handled similar situations?" Not that I'm aware of.

"I want to ensure that the materials we use fully comply with ASME standards and do not compromise the safety or integrity of our systems."

Absolutely agree!
 
Status