I have aluminum wire lugs and wnat to connect 6 AWG wire that is copper. Is it ok to combine the two materials.
 
Replies continue below

Recommended for you

Depends on the UL listing of the lugs. If they're listed or stamped "CU/AL" or similar, then you're set. If they're not listed or stamped as such, then you're out of luck.
 