Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Copper Alloys

Status
Not open for further replies.

soupy1957

Mechanical
Joined
Nov 23, 2005
Messages
23
I've got a Copper Alloy designation on a print that is identified as "A-35102 / Type L" and I was asked to tell the boss what alloy of Copper this was.
Since there are numerous Cu (Copper) alloys out there, ranging anywhere from "C80100" thru "C99750" I don't know what to tell him.
Any help identifying the correct alloy for "A-35102 / Type L" would be appreciated.
-Soupy1957
 
Last time I checked, the Copper Development Association (copper.org) would be happy to bury you in technical literature.



Mike Halloran
Pembroke Pines, FL, USA
 
Your designation A-35102 / Type L appears more like a part number off of a print for a component. What is the item?
 
There is a Type L Copper tubing under ASTM B88.
 
So far, what I've learned is that C221000 is the proper composition callout for the "L" designation Copper description.
The part, (as "metengr asks) is a copper tube.
-soupy1957
 