Convert Knoop to Vickers

Status
Not open for further replies.

9two5

Automotive
Oct 1, 2003
5
Does anyone know the formula for converting knoop to vickers. I am using a 500 gram load. I have charts, but they are not complete. Thanks in advance.
 
Replies continue below

Recommended for you

Thanks for the help, ASTM E140 was what I was looking for.
 