Hey guys, got a test result back and they gave it in lbs/in and I need it in N/mm as the requirement states. This is a breaking strength test for fabrics. I'm having a little trouble converting this, could anyone help me out? It is 88lbs/in
 
Replies continue below

Recommended for you

Wikipedia should have something comprehensive for this. I have a handy conversion program that I will post here when I find it.

BTW, units are never pluralized; e.g., 'lbs' is a no-no.

 