Jan 1, 2017 #1 ScottyUK Electrical Joined May 21, 2003 Messages 12,915 Location DE Interesting movie for anyone in the civil or oil industries. http://movingimage.nls.uk/film/5973
Jan 6, 2017 #2 ornerynorsk Industrial Joined Feb 5, 2002 Messages 3,198 Location US That's quite an interesting bit, even for those of us not in related fields. Thanks! It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all. Upvote 0 Downvote
That's quite an interesting bit, even for those of us not in related fields. Thanks! It is better to have enough ideas for some of them to be wrong, than to be always right by having no ideas at all.
Jan 6, 2017 #3 LittleInch Petroleum Joined Mar 27, 2013 Messages 23,022 Location GB Those gravity concrete structures of the 1970's were something else. The real fun is coming now as people try and either keep them going or wonder what to do with them because they aren't going to be re-floated.... The cormorant alpha platforms were rather big as well http://www.sir-robert-mcalpine.com/projects/index-thumbnailIndex=1&id=2523.html Remember - More details = better answers Also: If you get a response it's polite to respond to it. Upvote 0 Downvote
Those gravity concrete structures of the 1970's were something else. The real fun is coming now as people try and either keep them going or wonder what to do with them because they aren't going to be re-floated.... The cormorant alpha platforms were rather big as well http://www.sir-robert-mcalpine.com/projects/index-thumbnailIndex=1&id=2523.html Remember - More details = better answers Also: If you get a response it's polite to respond to it.
Jan 21, 2017 #4 EdStainless Materials Joined May 20, 2004 Messages 16,367 Location Waukesha WI USA I have seen (but can't find) footage of Phillips raising Ekofisk after it settled a 'little'. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
I have seen (but can't find) footage of Phillips raising Ekofisk after it settled a 'little'. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Jan 23, 2017 #5 Compositepro Chemical Joined Oct 22, 2003 Messages 7,846 Location US I very much enjoyed watching a program about the construction of the Troll gas platform quite a few years ago. https://www.youtube.com/watch?v=se26Ux9QD44 Upvote 0 Downvote
I very much enjoyed watching a program about the construction of the Troll gas platform quite a few years ago. https://www.youtube.com/watch?v=se26Ux9QD44