Hi, I have two new pads. One very large 100'x25' and one smaller square shape pad about 15'x15'. Both are 18" thick. The way they are oriented (see below), I am sure they would crack along their connected edge if they were poured together. Should I pour them as separate pads? I planned for it to be separate pads but it was brought up that it would cost a bit more construction wise. Is there a structural reason to justify the additional construction cost? Is there any issues if I go with a construction joint and it does end up cracking there?