I am looking at the Vulcraft catalog for Conform Metal Deck. The table states ( N=9 Normal Weight Concrete (145 PCF) What is N=9 ?
 
Replies continue below

Recommended for you

It's the ratio between the Modulus of Elasticity of steel (29,000,000 psi) to the Modulus of Elasticity of Concrete (~3,400,000 psi). It's normally rounded to an even number.
 
Or Bicycle?