Does anyone know of a source, besides Dupont, for static-dissipative PFA for melt extrusion ?
 
one of the companies I know is UPM in Raamsdonksveer in the netherlands ( Mr. Ed van Gilst ); this cie is a compounder for PTFE / PFA etc.
best regartds,
Ernst
 
LNP is another company, similar to RTP that does custom blends of materials.

considering conduction can be done with carbon fiber or graphite, and both of these are added to plastics regularly for wear resistance or minimizing thermal expansion, you might want to look at additional custom wear blenders.
 