Found this in a 50# condensate pipe run. Any ideas on the damage mechanism? It's carbon steel pipe.

-Mike
 
I assume it is pitting corrosin in the photo? if so CO2 is likely the corrodent. You will need to vent the non-condensibles or provide additional amine inhibitors.
 
Or is it blistering? What does it look like lightly cleaned?

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Rounded pits with steep walls, I woulg agree looks like CO2 pitting, have water in your condensate accumulating/condensing here.
 
Was just curious (for a little bit more info), what was the "clock" orieentation of this damage?
 