Does anyone have experience with concrete slabs that have the fiber mesh fibers sticking through the top of the slab, and how to remove them?
 
Replies continue below

Recommended for you

When Fibers became common, quite a few years ago, a building inspector (with a sly look) suggested an oversized safety razor.
 
I have not seen it done, but I hear people burn the exposed fibers with a torch
 
I have heard about the torch method as well…
 
If they are plastic fibre, torch. If they are steel fibre, top coat/leveling mix.
 
Turn'n Burn. Agree with CE here. The steel fibers will rust and stain the slab if not protected. Cleaning agents feed on steel.

Mike McCann, PE, SE (WA)


 
Also...use a hand-held roofing torch for modified bitumen membrane application. Can do a whole slab in a few minutes.
 
Fuzzy thinking leads to the use of plastic fibres in concrete, so fuzz in the finish is to be expected.
 