I have a one-story building with concrete-slab floor on grade, with carpet flooring. The slab is approximately 40-years old. Recently one corner of the concrete-slab floor (by the exterior walls) shows sign of surface delamination/flaking. Any idea what may cause that after 40-years.
 
 https://files.engineering.com/getfile.aspx?folder=d7be724c-94f8-4ab6-a19c-69f129dd7051&file=IMG_3007.JPG
Replies continue below

Recommended for you

Looks to me like levelling compound which has delaminated.
 