blowhard
Mechanical
- Dec 30, 2004
- 2
We are planning to add two new 12" SCH 40, CS laterals to an existing 24" RCP. Is there a limitation on the hole size that can be bored in a 24" pipe?
The laterals are dischrge lines from two new oily water separators. We don't have adquate spacing for a box and manhole at the tie-in points because of other underground lines in the area.
We plan to bore the 13.75" holes at 45 degrees and grout them in. Then build a form and pour concrete around the laterals for strength.
Any other suggestions? Thanks.
The laterals are dischrge lines from two new oily water separators. We don't have adquate spacing for a box and manhole at the tie-in points because of other underground lines in the area.
We plan to bore the 13.75" holes at 45 degrees and grout them in. Then build a form and pour concrete around the laterals for strength.
Any other suggestions? Thanks.