Agree with the previous posts, and Dr Lymon Reese, out of Texas, is by far the leading expert in the field.
We caught a contractor placing concrete with heavy renforcement (bundles of #8 rebar, etc) in 4 foot diameter piles for a landslide mitigation where he dropped concrete 75 feet (against our recommendation of no more than 5 feet). We actually cored the middle of a couple piles and drilled a couple pilot holes where we cored laterally.
Much to our surprise we found no honeycombing, especially in the outer raches where we expected to see signs of voids or disaggregation.
Regardless we would never recommend such a practice with rebar cages, but it was interesting to see.